Managing the use of copper-based antifouling paints M Srinivasan, GW Swain Environmental Management 39, 423-441, 2007 | 232 | 2007 |
The testing and evaluation of non‐toxic antifouling coatings GW Swain, MP Schultz Biofouling 10 (1-3), 187-197, 1996 | 203 | 1996 |
The influence of biofilms on skin friction drag MP Schultz, GW Swain Biofouling 15 (1-3), 129-139, 2000 | 187 | 2000 |
The development of microfouling on four commercial antifouling coatings under static and dynamic immersion F Casse, GW Swain International biodeterioration & biodegradation 57 (3), 179-185, 2006 | 180 | 2006 |
Adhesion Strength of Settled Spores of the Green Alga Enteromorpha JA Finlay, ME Callow, MP Schultz, GW Swain, JA Callow Taylor & Francis Group 18 (4), 251-256, 2002 | 176 | 2002 |
Bioinspiration—the solution for biofouling control? E Ralston, G Swain Bioinspiration & biomimetics 4 (1), 015007, 2009 | 163 | 2009 |
The use of proactive in-water grooming to improve the performance of ship hull antifouling coatings M Tribou, G Swain Biofouling 26 (1), 47-56, 2010 | 152 | 2010 |
The effect of biofilms on turbulent boundary layers MP Schultz, GW Swain | 144 | 1999 |
Surface elastic modulus of barnacle adhesive and release characteristics from silicone surfaces Y Sun, S Guo, GC Walker, CJ Kavanagh, GW Swain Biofouling 20 (6), 279-289, 2004 | 129 | 2004 |
Diatom community structure on commercially available ship hull coatings KA Zargiel, JS Coogan, GW Swain Biofouling 27 (9), 955-965, 2011 | 128 | 2011 |
Static vs dynamic settlement and adhesion of diatoms to ship hull coatings KA Zargiel, GW Swain Biofouling 30 (1), 115-129, 2014 | 121 | 2014 |
The effects of silicone fluid additives and silicone elastomer matrices on barnacle adhesion strength CJ Kavanagh, GW Swain, BS Kovach, J Stein, C Darkangelo-Wood, ... Biofouling 19 (6), 381-390, 2003 | 120 | 2003 |
Hydrodynamic forces on barnacles: Implications on detachment from fouling‐release surfaces MP Schultz, CJ Kavanagh, GW Swain Biofouling 13 (4), 323-335, 1999 | 118 | 1999 |
Silicone foul release coatings: effect of the interaction of oil and coating functionalities on the magnitude of macrofouling attachment strengths J Stein, K Truby, CD Wood, J Stein, M Gardner, G Swain, C Kavanagh, ... Biofouling 19 (S1), 71-82, 2003 | 116 | 2003 |
Structure-property relationships of silicone biofouling-release coatings: effect of silicone network architecture on pseudobarnacle attachment strengths J Stein, K Truby, CD Wood, M Takemori, M Vallance, G Swain, ... Biofouling 19 (2), 87-94, 2003 | 105 | 2003 |
Observations of barnacle detachment from silicones using high-speed video CJ Kavanagh, RD Quinn, GW Swain The Journal of Adhesion 81 (7-8), 843-868, 2005 | 104 | 2005 |
Redefining antifouling coatings G Swain Journal of Protective Coatings and Linings 16, 26-35, 1999 | 99 | 1999 |
The influence of biofouling adhesion and biotic disturbance on the development of fouling communities on non‐toxic surfaces GW Swain, WG Nelson, S Preedeekanit Biofouling 12 (1-3), 257-269, 1998 | 96 | 1998 |
Measuring the performance of today’s antifouling coatings GW Swain, B Kovach, A Touzot, F Casse, CJ Kavanagh Journal of Ship Production 23 (03), 164-170, 2007 | 93 | 2007 |
Two silicone nontoxic fouling release coatings: Hydrosilation cured PDMS and CaCO3 filled, ethoxysiloxane cured RTV11 KJ Wynne, GW Swain, RB Fox, S Bullock, J Uilk Biofouling 16 (2-4), 277-288, 2000 | 86 | 2000 |